Categories | WCu Alloy |
---|---|
Brand Name: | Hypersolid Metal |
Place of Origin: | China |
MOQ: | Negotiate |
Price: | Negitionable |
Payment Terms: | L/C, D/A, D/P, T/T, Western Union, MoneyGram |
Supply Ability: | 10000sets/month |
Delivery Time: | 30 days after receiving down payment |
Packaging Details: | Standard export cartons |
Meltingpoint: | 1495℃ |
Fracturetoughness: | 2.5 MPa·m1/2 |
Alloy Type: | WCu |
Tensile Strength: | 800-1000 MPa |
Melting Point: | 3420°C |
Density: | 15.63 g/cm3 |
Thermal Conductivity: | 180-200 W/m·K |
Material: | Tungsten Copper Alloy |
1,Description:
Material: Tungsten copper alloy plates are composed of a mixture of tungsten and copper. The alloy combines the high strength and thermal conductivity of tungsten with the excellent electrical conductivity of copper.
Composition: Tungsten copper alloy plates typically have a tungsten content ranging from 70% to 90%, with the remaining portion being copper. Different compositions can be tailored to meet specific requirements for thermal and electrical properties.
High Strength: Tungsten copper alloy plates exhibit high strength and hardness, making them suitable for applications requiring resistance to wear, deformation, and high mechanical stresses.
Thermal Conductivity: Tungsten copper alloy plates possess good thermal conductivity, allowing for efficient heat dissipation and thermal management in various applications.
Electrical Conductivity: Tungsten copper alloy plates have excellent electrical conductivity, making them suitable for electrical and electronic applications that require both high strength and good electrical performance.
2,Specifications:
Physical Property | Description |
---|---|
Composition | Tungsten and copper alloy |
Tungsten Content | 70% - 90% |
Copper Content | 10% - 30% |
Density | 14.0 - 16.5 g/cm³ |
Hardness | 200 - 400 HB (Brinell Hardness) |
Thermal Conductivity | 180 - 230 W/m·K |
Electrical Conductivity | 25 - 90% IACS (International Annealed Copper Standard) |
Coefficient of Thermal Expansion | 6.5 - 9.0 x 10^-6 /K |
![]() |